Results for "first layer height"
2 articles found
Textured PEI first-layer failures are ranked by frequency: fingerprint oils about 60%, worn texture 20%, wrong first-layer height 15%, and bed temperature too
Warping occurs when the bottom layer cools and contracts faster than the layers above it, lifting corners off the bed. Fix order: chamber temperature, bed